Abstract

Aseptic loosening due to osteolysis in total hip replacement has been related to wear debris released from prosthetic components. Retrospective long-term observations of patients with the metal-on-metal prosthesis has shown long-term survivorship and good mechanical performance. Thus, the new and modified metal-on-metal prosthesis has been introduced on the market. Historical clinical data from the 1 st generation metal-on-metal hip prosthesis may not be relevant for the 2nd generation of metal-on-metal hip prosthesis. Therefore, preclinical testing of the prosthesis must be conducted before clinical evaluation. We assessed the tribological performance of the metal-on-metal prosthesis versus the metal-on-polyethylene prosthesis introduced on the market as Metasul™ and Protasul™, respectively. In a 12-channel joint simulator, 6 metal-on-metal bearing and 3 metal on polyethylene prostheses were tested, with the same number of corresponding soak controls. The wear was assessed gravimetrically. The “steady-state” wear-rates from the metal-on-metal prosthesis were almost 100 times less than that from the metal-on-polyethylene prosthesis. The tribological wear performance of the metal-on-metal hip prosthetic system is promising.

Downloads

Download data is not yet available.

Downloads

Published

1999-01-01

How to Cite

Anissian, H. L., Stark, A., Gustafson, A., Good, V., & Clarke, I. C. (1999). Metal-on-metal bearing in hip prosthesis generates 100-fold less wear debris than metal-on-polyethylene. Acta Orthopaedica, 70(6), 578–582. https://doi.org/10.3109/17453679908997845